M. Holland Company LL102 LLDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company LL102 LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.3Processing Method: Blown FilmInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 440 %
440 %
ASTM D882
Film Elongation at Break, TD 580 %
580 %
ASTM D882
Secant Modulus, MD 0.255 GPa
37.0 ksi
1% Strain; ASTM D882
Secant Modulus, TD 0.317 GPa
46.0 ksi
1% Strain; ASTM D882
Coefficient of Friction 0.13
0.13
ASTM D1894
Dart Drop Test 130 g
0.287 lb
ASTM D1709
Film Tensile Strength at Break, MD 29.6 MPa
4300 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
Processing Properties Metric English Comments
Melt Temperature 182 - 221 °C
360 - 430 °F
Blow-up Ratio (BUR) 1.5 - 2.5
1.5 - 2.5
Descriptive Properties Value Comments
Form Pellets