M. Holland Company LD400 LDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company LD400 LDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High ESCR (Stress Crack Resist.), Good Processability, Low Temp. StrengthUses: Closures, Electrical Parts, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 2.3Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Yield 9.51 MPa
1380 psi
ASTM D638
Elongation at Break 480 %
480 %
ASTM D638
Tensile Modulus 0.169 GPa
24.5 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Descriptive Properties Value Comments
Form Pellets