Material Notes:
Features: High ESCR (Stress Crack Resist.), Good Processability, Low Temp. StrengthUses: Closures, Electrical Parts, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 2.2Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Tensile Modulus 0.165 GPa
24.0 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Descriptive Properties Value Comments
Form Pellets