Material Notes:
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, High Clarity, High Gloss, Heat Sealable, Good Processability, Medium SlipUses: FilmProcessing Method: Blown FilmInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.221 GPa
32.1 ksi
1% Strain; ASTM D882
Secant Modulus, TD 0.248 GPa
36.0 ksi
1% Strain; ASTM D882
Coefficient of Friction 0.12
0.12
ASTM D1894
Dart Drop Test 65.0 g
0.143 lb
ASTM D1709
Optical Properties Metric English Comments
Haze 5.5 %
5.5 %
ASTM D1003
Gloss 66 %
66 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
Blow-up Ratio (BUR) 1.5 - 2.5
1.5 - 2.5
Descriptive Properties Value Comments
Form Pellets