Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company LD220MM LDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company LD220MM LDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 2.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.152 GPa
22.0 ksi
1% Secant; ASTM D882
Coefficient of Friction >= 0.60
>= 0.60
ASTM D1894
Dart Drop Test 60.0 g
0.132 lb
Method F; ASTM D1708/A
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 40 %
40 %
at 45°; ASTM D2457
Descriptive Properties Value Comments
Form Pellets
Users viewing this material also viewed the following: