Material Notes:
Uses: Audio Tapes, Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3300 psi
Type I, 2 in/min; ASTM D638
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
at 0.05 in/min; ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.7 °C
197 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets