Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company CP503 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company CP503 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact copolymerGood impact resistanceLow temperature impact resistanceApplications: Compounding
Physical Properties Metric English Comments
Specific Gravity 0.903 g/cc
0.903 g/cc
23/23°C; ASTM D792
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 0.931 GPa
135 ksi
Procedure A; ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
73°F; ASTM D256
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding
Copyright © lookpolymers.com All Rights Reserved