M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
23/23°C; ASTM D792
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C

@Thickness 3.17 mm
170 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding