Material Notes:
Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Household Goods, Packaging Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 0.080 g/10 min
0.080 g/10 min
Condition G; ASTM D1238
1.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
Elongation at Break 3.4 %
3.4 %
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 4.48 J/cm
8.40 ft-lb/in
at 73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
0.250 in; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
0.250 in; ASTM D648
Descriptive Properties Value Comments
Form Pellets