Material Notes:
Medium flowMedium impact resistanceGood stiffnessInformation provided by M. Holland
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
23/23°C; ASTM D792
Melt Flow 14 g/10 min

@Load 10.0 kg,
Temperature 290 °C
14 g/10 min

@Load 22.0 lb,
Temperature 554 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C

@Thickness 6.35 mm
220 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Extrusion