Material Notes:
GUARD DOGâ„¢ UV292 is a highly effective hindered amine light stabilizer that protects polymers against degradation caused by exposure to UV radiation.Applications: This UV stabilizer is mainly used in Liquid Color Concentrates, Coatings, Printing Ink, Polyolefins, Polyurethane, Sealants, Adhesives, Elastomers, Unsaturated Polyesters, Acrylics and Styrenics. This stabilizer prevents automotive coatings from blowing-out and surface peeling. Also it is found to have a synergistic effect when used in combination with benzotriazole-type UV absorbers.Typical Properties: Product Form - Pale yellow liquid
Physical Properties Metric English Comments
Specific Gravity 0.9925 g/cc

@Temperature 20.0 °C
0.9925 g/cc

@Temperature 68.0 °F
Solubility >= 0.10 ppm
>= 0.10 ppm
Water
Molecular Weight 369.54 g/mol
369.54 g/mol
C<sub>21</sub>H<sub>39</sub>NO<sub>4</sub>
508.8 g/mol
508.8 g/mol
C<sub>30</sub>H<sub>56</sub>N<sub>2</sub>O<sub>4</sub>
Thermal Properties Metric English Comments
Melting Point 19.0 - 21.0 °C
66.2 - 69.8 °F
Boiling Point 220 °C

@Pressure 0.0000267 MPa
428 °F

@Pressure 0.00387 psi
Flash Point >= 150 °C
>= 302 °F
Ignition
Optical Properties Metric English Comments
UV Transmittance >= 97 %

@Thickness 0.425 mm
>= 97 %

@Thickness 0.0167 in
10g/100ml of Toluene
>= 99 %

@Thickness 0.500 mm
>= 99 %

@Thickness 0.0197 in
10g/100ml of Toluene
Descriptive Properties Value Comments
CAS Number 41556-26-7 & 82919-37-7
Molecular Formula C30H56N2O4 & C21H39NO4
Name Bis-(1,2,2,6,6-pentamethyly-4-piperdyl) sebacate & Methyl 1,2,2,6,6-pentamethyl-4 piperdyl sebacate
Recommended Dosage 1 - 2%
depending upon the substrate and performance requirements