Material Notes:
Data provided by Solvay Engineered Polymers.An engineered polyolefin designed for exterior painted automotive applications requiring dimensional stability over a broad temperature range. This material exhibits excellent low-temperature processability and properties.Uses: Bumper side claddings, rockers, and other components requiring close dimensional tolerances.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0065 cm/cm
0.0065 in/in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Ultimate 14.0 MPa
2030 psi
IV, 2 in/min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
I.B., TAN, 0.5 in/min; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
Modified; ASTM D696