LyondellBasell SEQUEL® 1825 Engineered Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer LyondellBasell
Trade Name SEQUEL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell SEQUEL® 1825 Engineered Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1825 engineered polyolefin is designed for automotive applications that require energy management combined with ductility and a balance of stiffness and impact resistance over a broad temperature range. This material provides excellent processability and dimensional stability. Applications: Body panels, bumper beams, energy absorbers, and brackets Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
as molded; ISO 294
Melt Flow 15 g/10 min
15 g/10 min
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 2.03 GPa
294 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 15.0 J
11.1 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 20.0 °C
30.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696