LyondellBasell Purell® PE3220D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Purell®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Purell® PE3220D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Purell PE 3220 D is a low density polyethylene with high rigidity and good chemical resistance. It is delivered in pellet form. Target markets are packaging of pharmaceuticals in the small blow molding market. Regulatory Status: Purell PE 3220 D meets the requirements of the Food and Drug Administration, Code of Federal Regulations, 21CFR Section 177.1520. This regulation allows the use of this olefin polymer in "articles or components of articles intended for use in contact with food." Contact your Equistar sales representative for more information regarding the suitability of specific products for specific applications. Specific recommendations for processing Purell PE 3220 D can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D638
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 660 %
660 %
ASTM D638
Tensile Modulus 0.483 GPa
70.0 ksi
1% Secant; ASTM D638
Flexural Modulus 0.494 GPa
71.6 ksi
1% Secant; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 48.0 °C
118 °F
ASTM D648
Vicat Softening Point 107 °C
225 °F
ASTM D1525