Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: good impact and stiffness balance, good cold impact resistance, excellent dimensional stability, FDA acceptableApplications: corrugated board extrusion, appliancesMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax SV258 medium impact polypropylene copolymer resin is suited for extrusion applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256A
Impact Test 31.0 J

@Temperature 5.00 °C
22.9 ft-lb

@Temperature 41.0 °F
Montell drop weight impact strength
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Users viewing this material also viewed the following: