LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation sterilization, easily processedApplications: medical devices, syringes, test tubes, blood vialsPassed USP Class VI testing. All ingredients meet TSCA (US) and DSL (Canada).Description: Pro-fax PF511 polypropylene homopolymer resin is designed for thermoformed container applications that require see-through clarity and good stiffness. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 74
74
ASTM D785A
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 16 %
16 %
ASTM D638
Flexural Modulus 0.780 GPa
113 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.330 J/cm
0.618 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648