Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-fax PD702NW Polypropylene Homopolymer, Nucleated/Antistat

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax PD702NW Polypropylene Homopolymer, Nucleated/Antistat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Injection MoldingKey Features: nucleated and antistatic, high flow polypropylene homopolymer resin, FDA acceptable, short cycle time for high productivity, resists dust pickup, enhanced stiffness, good flow propertiesApplications: large articles, thin wall partsMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax PD702N nucleated, antistatic, high flow, controlled rheology polypropylene homopolymer resin is designed for injection molding. It is available in pellet form. It meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785A
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved