LyondellBasell Pro-fax 7531 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 7531 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Injection Molding/ThermoformingKey Features: medium impact polypropylene copolymer resin for food packaging, FDA acceptable, low odor and low taste transfer, good cold impact resistance, excellent dimensional stabilityApplications: food containers, medical wares, housewaresMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax 7531 medium impact polypropylene copolymer resin is designed for food packaging applications. It can be used on standard injection molding and thermoforming equipment. It has passed USP Class VI testing. It has a yellow card RTI, which applies to all colors. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256A
Impact Test 26.0 J

@Temperature -29.0 °C
19.2 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
UL RTI, Mechanical with Impact 65.0 °C
149 °F
Minimum thickness 0.039 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.039 inches.