LyondellBasell Pro-fax 6331NW Polypropylene Homopolymer, Nucleated/Antistat

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 6331NW Polypropylene Homopolymer, Nucleated/Antistat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: antistatic and nucleated polypropylene homopolymer resin, short cycle time, resists dust pickup, low odorApplications: lightweight containers, closures, hospital and institutional ware, toysMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax 6331NW polypropylene homopolymer resin is nucleated for faster crystallization and features antistatic properties. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. It has a UL yellow card RTI, which apply to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785A
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.460 J/cm
0.862 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ASTM D648
UL RTI, Mechanical with Impact 65.0 °C
149 °F
Minimum thickness 0.038 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.038 inches.