LyondellBasell Petrothene® PM92973 Linear Low Density Polyethylene Black Concentrate

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® PM92973 Linear Low Density Polyethylene Black Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE PM 92973 is a black concentrate formulated to be used with PETROTHENE GA 808-091, a natural LLDPE let-down resin, for use in the extrusion of communications and power cable jacketing. Antioxidant, to ensure long-term stability, and a processing aid have been added. This resin can be successfully used with LLDPE, MDPE, HDPE and PP resins.Processing TechniquesPM 92973 should be let down at a ratio of 14.4:1 to yield the optimum 2.6% final carbon black loading. PM 92973 is 6.5% of the final product.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D1505
Carbon Black Loading 40 %
40 %