Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Blow Molding)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Blow Molding).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 345-009 is a low density homopolymer resin designed for blow molding applications. Excellent clarity combined with strength and high stiffness makes NA 345-009 an ideal choice for flexible containers, squeeze bottles and toys. Regulatory StatusNA 345-009 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 345-009 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.9205 g/cc
0.03326 lb/in³
ASTM D1505
Melt Flow 1.8 g/10 min
1.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 0.296 GPa
43.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C
115 °F
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746