Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer "...in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing NA272130 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238
Antiblock Level 1000 ppm
1000 ppm
Slip Level 300 ppm
300 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Dart Drop 1.57 g/micron
40.0 g/mil
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 24.1 MPa
3500 psi
ASTM D882
Film Tensile Strength at Break, TD 20.7 MPa
3000 psi
ASTM D882
1% Secant Modulus, MD 331 MPa
48000 psi
ASTM D882
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 90 %
90 %
60°; ASTM D523