LyondellBasell Petrothene® NA216000 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA216000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 216-000 is a general purpose, heavy and medium weight coating resin, capable of coating weights down to 7.0 lbs/ream at line speeds of 1200 ft/min. It can be applied to paper, foil, cellophane, polyester film, and other base stocks by the conventional extrusion coating process. Products made from materials coated with NA 216-000 include flexible packaging milk cartons, set-up cartons and food boards and other materials. Regulatory StatusNA 216-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesThe maximum recommended melt temperature for NA 216-000 is 625°F. For further suggestions, contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 3.7 g/10 min
3.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength at Break 12.1 MPa
1750 psi
Type IV specimen; ASTM D638
Elongation at Break 550 %
550 %
Type IV specimen; ASTM D638
Flexural Stiffness 276 MPa
40000 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525