LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Sheet/Profile extrusions
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. Regulatory Status: NA149000 meets the requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of this olefin polymer in "...articles or components of articles intended for use in contact with food;" or "as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing NA149000 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa
1590 psi
ASTM D638
Elongation at Yield 640 %
640 %
ASTM D638
1% Secant Modulus 198 MPa
28700 psi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<SUB>50</SUB>; ASTM D746