Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® LB500301 High Density Polyethylene, Blow Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® LB500301 High Density Polyethylene, Blow Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PETROTHENE LB500301 is a polyethylene resin that exhibits excellent environmental stress crack resistance and is especially designed for heavy duty bottles, such as those containing detergent and chemicals.Regulatory Status: LB500301 meets the requirements of the Food and Drug Administration, regulation 21 CFR 1 77.1 520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information about the use of specific products for specific applications.Specific recommendations for processing LB500301 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
ESCR 100% Igepal® 75 hour
75 hour
F<SUB>50</SUB>; CO-630; ASTM D1693
>= 500 hour
>= 500 hour
F<SUB>50</SUB>; ASTM D2561
Melt Flow 0.30 g/10 min
0.30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Tensile Impact 64.1 J/cm
120 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746