LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogeneity, require no transfer equipment modifications, and facilitate clean and safe handling. Applications include heavy duty shipping sacks, prime liners, commercial and industrial packaging, as well as food and consumer packaging. Processing TechniquesRecommended processing conditions for the GA 601 series are a 400°-450°F melt temperature and a 1.5-3.01:1 blow-up ratio. Using proper techniques, this product can readily be drawn below 0.9 mil at optimum production rates. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known. For further suggestions, please contact your Equistar sales representative. Regulatory StatusGA 601 series resins meet the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Physical PropertiesTHE GA 601 series resins offer enhanced film strength, drawdown, toughness and heat seal strength. In addition, they have excellent low temperature resistance for applications such as stretch film and frozen food packaging. The GA 601 series resins can be purchased without additives, fully formulated with slip and antiblock or containing a processing aid.Other InformationBlow-up ratio 2.5:1.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 38.1 microns
1.50 mil
2.5:1 BUR
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 625 %
625 %
ASTM D882
Dart Drop, Total Energy 2.44 J
1.80 ft-lb
ASTM D4272
Elmendorf Tear Strength MD 600 g
600 g
ASTM D1922
Elmendorf Tear Strength TD 900 g
900 g
ASTM D1922
Dart Drop Test 290 g
0.639 lb
F<sub>50</sub>; ASTM D1709A
Film Tensile Strength at Break, MD 36.5 MPa
5300 psi
ASTM D882
Film Tensile Strength at Break, TD 29.0 MPa
4200 psi
ASTM D882
1% Secant Modulus, MD 207 MPa
30000 psi
ASTM D882
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 50 %
50 %
45°; ASTM D2457
Descriptive Properties Value Comments
Antiblock None
Slip None