LyondellBasell Montell 8640 Polybutene-1

Category Polymer , Thermoplastic , Polybutene
Manufacturer LyondellBasell
Trade Name Montell
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Montell 8640 Polybutene-1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements in 21 CFR 177.1570 for direct food contact up to 212°F (100°C).Description: Polybutene-1 PB 8640 is a semi-crystalline low ethylene content random copolymer which is miscible with polypropylenes due to its similar molecular structure. In blends with polyethylenes it is immiscible but easily dispersible. This copolymer is used in the packaging industry primarily as a minor additive in a polyethylene seal-peel layer for the production of coextruded flexible film or more rigid sheet. Varying the concentration in the seal-peel layer offers the unique possibility of tailoring the seal strength for controlled easy-opening of peelable seal packaging. This grade is particularly suitable for use in blown film formulations when low heat seal initiation temperatures are required. A typical blend partner is a high density polyethylene with a melt index range between 0.5 and 2 dg/min. This copolymer meets FDA requirements for direct food contact under regulation 21 CFR 177.1570.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.908 g/cc
0.0328 lb/in³
ASTM D1505
Melt Flow 1.0 g/10 min
1.0 g/10 min
ISO 1133-1981E
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 27.6 MPa
>= 4000 psi
ISO 1184-1983E
Tensile Strength, Yield 11.7 MPa
1700 psi
ISO 1184-1983E
Elongation at Break >= 350 %
>= 350 %
ISO 1184-1983E
Modulus of Elasticity 0.193 GPa
28.0 ksi
ISO 1184-1983E
Thermal Properties Metric English Comments
Melting Point 116 °C
241 °F
DSC
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746