Material Notes:
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferApplications: wear surfaces in pulp and paper process, material handling and packaging equipment, food and beverage processing systems, impact and abrasion resistant parts for mining and solid waste handling, marine fendering, battery separators, FDA acceptableMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: 1900 ultrahigh molecular wight polyethylene resin has an average molecular weight range between 4 and 6 million. This polymer is for use in compression moldind, solution and ram extrusion processes. It is supplied in a fine powder form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. It has passed USP Class VI testing. This resin has passed the tesing for compliance with 3A Sanitary Standards for plastics in contact with dairy products. All indgredients meet the chemical regristration requirments of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Apparent Bulk Density 0.470 - 0.470 g/cc
0.0170 - 0.0170 lb/in³
ASTM D792
Viscosity Test 2600 cm³/g
2600 cm³/g
Intrinsic; ASTM D4020
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 0.750 GPa
109 ksi
1% secant at 0.05 in/min; ASTM D790B
Izod Impact Resistance 6.50 J/cm²
30.9 ft-lb/in²
ASTM D4020-98
Abrasion 7.7
7.7
% Abrasion Index; Montell P116 Test