LyondellBasell Lupolen® V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer LyondellBasell
Trade Name Lupolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolen® V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.00 MPa
1020 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 0.0650 GPa
9.43 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Melting Point 91.0 °C
196 °F
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Oxygen Index 19 %
19 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Dielectric Constant 2.6

@Frequency 100 Hz
2.6

@Frequency 100 Hz
Dissipation Factor 0.024

@Frequency 100 Hz
0.024

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V