LyondellBasell Hostacom™ ZG750 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacom™ ZG750 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacom™ ZG750 conventional melt flow, 1,700 MPa flexural modulus, 40% calcium carbonate-filled, utility grade polypropylene copolymer resin has a very good combination of strength, stiffness and impact resistance. Features include good impact/stiffness balance and good processability. Uses: Industrial applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527-1, -2
Elongation at Break 350 %
350 %
ISO 527-1, -2
Flexural Modulus 1.70 GPa
247 ksi
ISO 178
Izod Impact, Notched (ISO) 3.70 kJ/m²

@Temperature -30.0 °C
1.76 ft-lb/in²

@Temperature -22.0 °F
ISO 180
45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 23.0 J

@Temperature 23.0 °C
17.0 ft-lb

@Temperature 73.4 °F
Gardner Falling Dart Impact (GFDI); ASTM D5420