LyondellBasell Hostacomâ„¢ AE716BC Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ AE716BC Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacomâ„¢ AE716BC conventional melt flow, 1,400 MPa flexural modulus, UV-stabilized, 40% calcium carbonate-filled polypropylene homopolymer has a good balance of properties and processing. It was designed to meet UL 746B (F1) requirements for outdoor applications. Uses: Electrical parts, outdoor applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D 785
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D 638
Elongation at Yield 25 %
25 %
ASTM D 638
Flexural Modulus 1.40 GPa
203 ksi
procedure A; ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
Unannealed; ASTM D648