LyondellBasell Astryn BA66K Polypropylene Copolymer, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn BA66K Polypropylene Copolymer, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, high limiting oxygen index, non-halogenated, good aesthetics, excellent processabilityApplications: batteries, electrical componentsDescription: Astryn BA66K high melt flow, UL 94 V-2 flame tretardant polypropylene copolymer has an excellent cobination of properties and processability. It is non-halogenated and was designed for applications which have stringent flammability requirements.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Tool, Montell
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256A
Gardner Impact 3.00 J
2.21 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Oxygen Index 38 %
38 %
ASTM D2863