LyondellBasell Astryn BA16G Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn BA16G Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade polypropylene copolymer, good flexibility, high impact strength, good colorability, good processability, good weatherabilityApplications: weatherstripping, profilesDescription: Astryn BA16G fractional melt flow, UV-stabilized, extrusion grade polypropylene copolymer has a good balance of flexibility, impact resistance, colorability and processability. It was designed for extruded components which require long periods of outdoor service.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Tool, Montell
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 71
71
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 5.30 J/cm
9.93 ft-lb/in
ASTM D256A
Gardner Impact 11.0 J

@Temperature -30.0 °C
8.11 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648