LyondellBasell Astryn 75F4-2 Polypropylene Copolymer, 20% Talc

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn 75F4-2 Polypropylene Copolymer, 20% Talc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: conventional melt flow, medium high modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aestheticsApplications: small appliances, electrical components, housewaresDescription: Astryn 75F4-2 conventional melt flow, 20% talc-filled polypropylene copolymer has an excellent combination of strength, stiffness, impact resistance and colorability.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792B
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ASTM D785
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648