Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Astryn 6652 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn 6652 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: low melt flow, medium modulus polypropylene homopolymer, high strength, high impact, good hydrolytic abilityApplications: water pipe fittings and connectorsDescription: Astryn 6652 low melt flow, polypropylene homopolymer has high strength, excellent impact resistance and good hydrolytic stability.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792B
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 1.50 J/cm
2.81 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved