LyondellBasell Astryn 65F5-2 Polypropylene Homopolymer, 20% Calcium Carbonate

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn 65F5-2 Polypropylene Homopolymer, 20% Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: conventional melt flow, medium high modulus, mineral-filled polypropylene homopolymer, high stiffness, excellent chemical resistance, good surface qualityApplications: automotive components, small and large appliances, housewaresDescription: Astryn 65F5-2 conventional melt flow, 20% calcium carbonate-filled polypropylene homopolymer is designed for high stiffness, excellent chemical resistance and improved surface quality of molded parts.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792B
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ASTM D785
Tensile Strength, Ultimate 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ASTM D648