Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5045 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5045 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 5045 is a medium molecular weight high density polymer for use in blown film extrusion applications. Typical applications include millinery bags, coextrusions and plastic netting.Regulatory StatusL 5045 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing L 5045 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Extrusion Condtions: BUR=2-2.5:1; Frost Line 24 inch; 1.0 Mil Film; Melt Temperature- 390-420°F(199-216°C)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Thickness 25.4 microns
1.00 mil
2 - 2.5 BUR; Frost line 24 inch
Melt Flow 0.45 g/10 min
0.45 g/10 min
ASTM D1238
Processing Properties Metric English Comments
Melt Temperature 199 - 216 °C
390 - 421 °F
Typical Extrusion