Lushan M-12A Adhesive Resin for Multi-layer Oxygen Barrier Pipe

Category Polymer , Adhesive , Thermoplastic , Polyolefin
Manufacturer Lushan
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lushan M-12A Adhesive Resin for Multi-layer Oxygen Barrier Pipe.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Adhesive resin Lushan series for multi-layer oxygen barrier pipe is a modified polyolefin with functional groups. It’s designed to bond to a variety of barrier materials, such as nylon and ethylene vinyl alcohol (EVOH) etc.Adhesive resin Lushan M-20A & 12A have goods properties as below: High bonding strengthA wide range of bondingExcellent chemical bonding with barrier materials EVOH & NylonExcellent heat resistance, weather resistance, chemical resistanceExcellent mechanical propertiesEasy processing for adhesive resinHygiene and safety, non-toxic residue for adhesive resin, etc.Applications: EVOHInformation provided by Lushan
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D1505
Melt Index of Compound 2.55 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.55 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 720 %
720 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 100.6 °C
213.1 °F
ASTM D1525
Processing Properties Metric English Comments
Moisture Content 0.060 %
0.060 %
HG/T2751
Descriptive Properties Value Comments
Appearance Transparent particles