Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP)
Manufacturer Lushan
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed for multi-layer sausages casing films composed of polyethylene (PE) and EVOH or PA. Lushan adhesive resins are based on LLDPE and are highly stabilized for multi-layer sausages casing films application in three layer casing film like PA/Tie layer resin/PA and five layer casing film like PA/Tie layer resin PE/Tie resin/PA. Lushan casing film adhesive resin created super adhesion between EVOH and PE while maintaining an excellent processability equivalent to that of common LLDPE. Adhesive resin Lushan series for food package complies with FDA 21CFR175.105 and suitable for indirect food contact.Application: TransparentInformation provided by Lushan
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D1505
Melt Index of Compound 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
ASTM D2117
Vicat Softening Point 70.0 °C
158 °F
ASTM D1525
Brittleness Temperature -70.0 °C
-94.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Appearance Transparent particles