Lucobit Lucowax® 1705 Polyethylene Wax

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Lucobit AG
Trade Name Lucowax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucowax® 1705 Polyethylene Wax.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucowax is a polyethylene wax additive for the modification of bitumen or asphalt.The addition of Lucowax reduces viscosity and penetration, while increasing water resistance, plasticity, and deformation resistance.Information provided by Lucobit AG
Physical Properties Metric English Comments
Brookfield Viscosity 10 - 20 cP

@Temperature 135 °C
10 - 20 cP

@Temperature 275 °F
Thermal Properties Metric English Comments
Dropping Point 114 - 120 °C
237 - 248 °F
Metter 1°C/min
Descriptive Properties Value Comments
Congealing Point, °C 100 - 106
ASTM D 938
Needle Penetration, 1/10mm 0 - 12
at 65°C; ASTM D 1321
0 - 2
at 25°C; ASTM D 1321