Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Lucobit AG
Trade Name Lucofin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene homopolymers with comparable density.Information provided by Lucobit AG
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ISO 1183
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ISO 868
Tensile Strength, Yield 4.00 MPa
580 psi
ISO 527
Elongation at Yield 14.5 %
14.5 %
ISO 527
Modulus of Elasticity 0.0620 GPa
8.99 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
ISO 3146
Vicat Softening Point 70.0 °C
158 °F
ISO 306
Processing Properties Metric English Comments
Processing Temperature 160 - 190 °C
320 - 374 °F
Blown film
160 - 200 °C
320 - 392 °F
Profiles and hoses
160 - 200 °C
320 - 392 °F
Blow molding
160 - 230 °C
320 - 446 °F
Flat-sheet
160 - 270 °C
320 - 518 °F
Coatings