Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Cast
Manufacturer Lucite International
Trade Name Perspex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast method of manufacture is ideally suited to small colour runs and batch sizes.Information provided by Lucite International.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ISO 2039-2
Tensile Strength, Ultimate 75.0 MPa
10900 psi
5 mm/min; ISO 527
Elongation at Break 4.0 %
4.0 %
5 mm/min; ISO 527
Flexural Strength 116 MPa
16800 psi
2 mm/min; ISO 178
Flexural Modulus 3.21 GPa
466 ksi
2 mm/min; ISO 178
Charpy Impact Unnotched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 77.0 µm/m-°C

@Temperature 20.0 °C
42.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Vicat Softening Point >= 110 °C
>= 230 °F
ISO 306A
Flammability, UL94 HB
HB
Flammability Test 3.0
3.0
BS 476, Pt7
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489/A
Transmission, Visible >= 92 %
>= 92 %
clear grade; in 3 mm (colored grades lower); ASTM D1003