Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Lucite® 47 Glass Separation Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Lucite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Lucite® 47 Glass Separation Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improper storage and transport of glass products (e.g. flat glass or fabricated items) can lead to costly damage caused by glass-to-glass abrasion and/or corrosion rendering it unsuitable for end-use. Lucite® Acrylic Resins in combination with adipic acid provides excellent protection of glass during storage and shipment.The blend of adipic acid with Lucite® acrylic resins provides the following benefits: Prevents glass-to-glass abrasion/scratching; Prevents glass corrosion when blended with adipic acid; Physical separator to ease glass handling; Highly resilient; Inert, non-hazardous; Cost effective; Perfectly suited for automated glass handling/processing; Easy to apply; Easy to removeInformation provided by Lucite International
Physical Properties Metric English Comments
Water Absorption 0.30 %
0.30 %
Particle Size 130 - 170 µm
130 - 170 µm
Viscosity Measurement 0.40 - 0.60
0.40 - 0.60
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
Tensile Strength 73.0 MPa
10600 psi
Elongation at Break 4.0 %
4.0 %
Optical Properties Metric English Comments
Refractive Index 1.491
1.491
Transmission, Visible 92 %
92 %
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %
Users viewing this material also viewed the following: