Lucite International Elvacite ® 4409 Acrylic Resin, Hydroxyl Functional

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 4409 Acrylic Resin, Hydroxyl Functional.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 4409 is a solid methacrylate copolymer bead resin designed for use in formulating environmentally sound thermosetting coatings and adhesives. The resin may be used as the main binder in acrylic systems, or blended with other resins to improve weather resistance and clarity. Elvacite® 4409 is solvent free to provide maximum formulation latitude.Information provided by Lucite International
Physical Properties Metric English Comments
Viscosity Measurement 0.18
0.18
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 31000 g/mol
31000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 104 °C
219 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Descriptive Properties Value Comments
Hydroxyl Number 4