Material Notes:
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by injection molding or extrusion.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 0.36 %
0.36 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Melt Flow 3.7 g/10 min
3.7 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 30
30
ISO 2039-2
Tensile Strength 38.0 MPa
5510 psi
ISO 527
Elongation at Break 33 %
33 %
ISO 527
Flexural Strength 54.0 MPa
7830 psi
ISO 178
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 6.90 kJ/m²
3.28 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.780 J/cm²
3.71 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C
66.7 µin/in-°F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ISO 75A
Vicat Softening Point 82.0 °C
180 °F
ISO 306B
94.0 °C
201 °F
ISO 306A
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003