Material Notes:
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by injection molding or extrusion.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Water Absorption 0.32 %
0.32 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 4.8 g/10 min
4.8 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 69
69
ISO 2039-2
Tensile Strength 58.0 MPa
8410 psi
ISO 527
Elongation at Break 15 %
15 %
ISO 527
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 3.40 kJ/m²
1.62 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
4.20 J/cm²
20.0 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
ASTM E831
Vicat Softening Point 94.0 °C
201 °F
ISO 306B
104 °C
219 °F
ISO 306A
Heat Distortion Temperature 92.0 °C
198 °F
ISO 75A
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003