Lucite International Colacryl ® TS1742 Acrylic Dental Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS1742 Acrylic Dental Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucite® Colacryl® TS1742 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of heat-cured, soft materials, such as ear moulds, where it is well suited to use with Colacryl® TS1741 dental liquid.Information provided by Lucite International
Physical Properties Metric English Comments
Particle Size 35 - 55 µm
35 - 55 µm
Molecular Weight 300000 - 500000 g/mol
300000 - 500000 g/mol
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %
Descriptive Properties Value Comments
BPO Content (%) 0.6