Lucite International Colacryl ® LS600/1 Specialty Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® LS600/1 Specialty Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Colacryl® LS600/1 is a methyl methacrylate based acrylic resin with excellent resistance to water whitening in reactive systems. It is soluble in chlorinated hydrocarbons, ketones and lower esters and compatible with other methyl methacrylate resins and also with common plasticisers e.g. phthalates, citrates and sebacates.Typical applications include solid surfaces and adhesives.Information provided by Lucite International
Physical Properties Metric English Comments
Viscosity Measurement 2.5 - 3.0
2.5 - 3.0
reduced, 1% solution in chloroform; Ubbeholde "A" viscometer
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %