Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.021 cm/cm

@Thickness 3.17 mm
0.021 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.97 MPa
10000 psi
ASTM D638
Elongation at Break >= 20 %
>= 20 %
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.828 GPa
410.1 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.30 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 170 - 175 °C
338 - 347 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648