Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers PC/ABS-FR0 Polycarbonate+ABS, Flame Resistant

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers PC/ABS-FR0 Polycarbonate+ABS, Flame Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added Release, "U" for UV Stabilizer and "EF" for Easy Flow (35.0 g/10min)UL Listing: File No. E213588Information provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 260 °C
20 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.07 MPa
9003 psi
ASTM D638
Elongation at Break >= 40 %
>= 40 %
ASTM D638
Flexural Strength 102.07 MPa
14804 psi
ASTM D790
Flexural Modulus 2.586 GPa
375.1 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 101.67 °C
215.01 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Users viewing this material also viewed the following: